Polymer Property : Kinematic Viscosity at 100°C (212°F) = 31 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 31 cSt
31 cSt
Lubriplate APG-140 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..