Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 22 cSt
22 cSt
Lubriplate H0-5 Petroleum-Based Heavy-Duty Hydraulic Oil
Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin..
Kinematic Viscosity at 100°C (212°F) 22 cSt
22 cSt
ASTM D445
Solvay Specialty Polymers FOMBLIN® M15 PFPE Lubricant
Information provided by Solvay Solexis, Inc.