Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 66 SUS
66 SUS
Lubriplate AC-2A Petroleum-Based Air Compressor Fluid
Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar..
Saybolt Viscosity at 210°F 66 SUS
66 SUS
Lubriplate FMO 500 AW USP Mineral Oil-Based Food Machinery Grade Oil
For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps..
Saybolt Viscosity at 210°F 66 SUS
66 SUS
Lubriplate H0-2A Petroleum-Based Heavy-Duty Hydraulic Oil
Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin..
Saybolt Viscosity at 210°F 66 SUS
66 SUS
Lubriplate SYN LUBE 100 PAO-Based Multi-Purpose Synthetic Fluid
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for..