Polymer Property : Saybolt Viscosity at 210°F = 60 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 60 SUS
60 SUS
Lubriplate SYNAC 100 Diester-Based Synthetic Air Compressor Fluid
These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S..