Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 188 SUS | 188 SUS | |
Lubriplate SYN-H1-220 Polyalkylene Glycol-Based Synthetic Food Machinery Grade Fluid Specifically designed for use where elevated temperatures exist and the need for a food grade lubricant is required. For chain applications where air temperatures exceed 400°F and up to 600°F .. |