Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 99 cSt | 99 cSt | |
Lubriplate AC-2A Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 99 cSt | 99 cSt | |
Lubriplate FMO 500 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Kinematic Viscosity at 40°C (104°F) | 99 cSt | 99 cSt | |
Lubriplate H0-2A Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |