Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 497 cSt | 497 cSt | |
Lubriplate TEMP HIGH Bentone Type Multi-Purpose Grease For Special Conditions Multi-purpose, high temperature, bentone type grease workable from 40°F to 500°F.Applications: Multi-Purpose, high temp. applicationsHIGH TEMP is available in Cartridges, Cans, Pails, 1/4 Drum.. |