Polymer Property : Kinematic Viscosity at 40°C (104°F) = 446 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 446 cSt
446 cSt
Lubriplate SFGO Ultra-460 PAO-Based Synthetic Food Machinery Grade Fluid
Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi..
Kinematic Viscosity at 40°C (104°F) 446 cSt
446 cSt
Lubriplate SYN SYN-1602 PAO-Based Multi-Purpose Grease
Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w..