Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 25 cSt | 25 cSt | |
Lubriplate Low Pour Petroleum-Based Heavy-Duty Hydraulic Oil ISO 22 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate |