Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 19 cSt | 19 cSt | |
Lubriplate AERO Lithium Based Grease For Special Applications / Conditions Lithium based for cold temperature applications down to -60°F. Provides low-torque start-up capability, excellent corrosion & oxidation resistance and wide compatibility with metal, plastic, & ru.. |
|||
Kinematic Viscosity at 40°C (104°F) | 19 cSt | 19 cSt | |
Lubriplate FMO 85 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |