Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 144 cSt | 144 cSt | |
Lubriplate FML 0 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available .. |
|||
Kinematic Viscosity at 40°C (104°F) | 144 cSt | 144 cSt | |
Lubriplate FML 1 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available .. |
|||
Kinematic Viscosity at 40°C (104°F) | 144 cSt | 144 cSt | |
Lubriplate FML 2 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available .. |