Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 85 SUS | 85 SUS | |
Heatbath/Park AAA Quench Oil AAA Quench Oil is the most widely specified accelerated fast oil quenchant. It is ideal for carbon steel and low and medium alloy steel. AAA Quench Oil achieves faster cooling rates through intensi.. |