Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 490 SUS | 490 SUS | |
Lubriplate NO. 3 NO.3 Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |