Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 39.2 SUS
39.2 SUS
Heatbath/Park Plastiquench Water-Based Quenchant
A solution of polyvinyl alcohol in water, used as a base for steel quenching media. In water solution, it cools austenitized steels faster then quenching oils, hardens steels with less distortion or..