Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Saybolt Viscosity at 100°F = 36 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 36 SUS
36 SUS
Heatbath/Park Parquench 90 Water-Based Quenchant
The higher molecular weight polymer package. It is generally used for higher alloy steels and all types of metals where the control of distortion is of prime importance. Typical concentration is 15..
Copyright © lookpolymers.com All Rights Reserved