Polymer Property : Saybolt Viscosity at 100°F = 3.9 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 3.9 SUS
3.9 SUS
At 100°F in SUS; cSt
Heatbath/Park Polyquench 20 Water-Based Quenchant
Water solution of standard, "Type I", polyalkylene glycol quenchant. The polymer is inversely soluble above 1650°F. Typical concentration is 15%.Information provided by Heatbath Corporation - Pa..