Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 1112 SUS | 1112 SUS | |
Lubriplate 220 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity .. |