Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 508 µm | 508 µm | |
Mid-Mountain Materials SILTEX® XS-150 Silica Yarn SILTEX® SILICA YARN XS-150 is comprised of continuous filament, amorphous silica fibers and offers superior protection in electrical applications, as well as excellent resistance to thermal shock.. |