Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 400 µm | 400 µm | |
EMS-Griltech Grilamid® DM 10 Nylon 12 Monofilament Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |
|||
Filament Diameter | 400 - 500 µm | 400 - 500 µm | |
EMS-Griltech Grilon® XC 130 Nylon 610 Monofilament (Non-Set) Description: GRILON XC 130 is a Nylon 610 based monofilament for press felt fabric.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Filament Diameter | 400 µm | 400 µm | |
EMS-Griltech Grilon® XC 133 Nylon 610 Monofilament (Medium-Set) Description: GRILON XC 133 is a Nylon 610 based monofilament for press felt fabric.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |