Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 2.0 - 4.0 µm | 2.0 - 4.0 µm | |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Filament Diameter | 2.0 - 4.0 µm | 2.0 - 4.0 µm | |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Filament Diameter | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Zircar Refractory Composites RS-SI SILICA MOLDABLE ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid.. |