Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.60 g/cc | 9.60 g/cc | |
Plansee MoCu40 Molybdenum-Copper Characteristics:High thermal conductivityLow thermal expansionIdeal for heat dissipation applications related to: IGBT modules, RF packages, and LED chips, among others.Information provided by Plans.. |