Physical Properties Metric English Comments
Specific Gravity 9.34 g/cc
9.34 g/cc
Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy
Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joinin..
Specific Gravity 9.34 g/cc
9.34 g/cc
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy
Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s..