Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.29 g/cc | 9.29 g/cc | |
Lucas-Milhaupt Silvaloy® 35 Brazing Alloy Silvaloy 35 is an alloy with a melting range suitable for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is free-flowing and suited .. |