Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.11 g/cc | 9.11 g/cc | |
Lucas-Milhaupt Silvaloy® A45 Brazing Alloy Silvaloy A45 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in the electrical industry and for brazing .. |