Polymer Property : Specific Gravity = 9.00 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 9.00 g/cc
9.00 g/cc
ASTM D792
Ecomass® 1003ZD95 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Specific Gravity 9.00 g/cc
9.00 g/cc
ASTM D792
Ecomass® 1080ZD94 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn..