Polymer Property : Specific Gravity = 8.02 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 8.02 g/cc
8.02 g/cc
Crucible Steel 347 Chromium-Nickel Steel
Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..
Specific Gravity 8.02 g/cc
8.02 g/cc
Crucible Steel 348 Chromium-Nickel Steel
Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..