Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A) TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr.. |
|||
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Latrobe LSSâ„¢ A2 Tool Steel (ASTM A2) TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance be.. |
|||
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6) R.D.S. tool steel is an oil hardening die steel which combines extreme toughness with very little size change when heat treated. It is available as a DeCarb-Free product. DCF bars have been cold fin.. |
|||
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Carpenter Hampden® High Carbon, High Chrome Tool Steel (Oil-Wear) (AISI D3) Hampden tool steel is an oil-hardening, high-carbon, high-chromium die steel having extreme wear resistance, It hardens with very little change in size or shape. Hampden tool steel is a deep-hardeni.. |
|||
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Latrobe LSS™ L6 Tool Steel (ASTM L6) TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good .. |
|||
Specific Gravity | 7.86 g/cc | 7.86 g/cc | |
Latrobe LSS™ P20 Mold Steel (ASTM P20) TLS P20 mold steel is a versatile, low-alloy tool steel that is characterized by good toughness at moderate strength levels. The steel is commonly used for plastic injection mold cavities and toolin.. |