Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.81 g/cc | 7.81 g/cc | |
Latrobe Whitebear® Cold Work Tool Steel (ASTM A18) Whitebear cold work tool steel is a versatile air-hardening tool steel in the 8% chromium family that is characterized by a very good combination of toughness and wear resistance. It contains lower .. |
|||
Specific Gravity | 7.81 g/cc | 7.81 g/cc | |
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho.. |
|||
Specific Gravity | 7.81 g/cc | 7.81 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |