Polymer Property : Specific Gravity = 7.761 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 7.761 g/cc
7.761 g/cc
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti..