Polymer Property : Specific Gravity = 7.76 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 7.76 g/cc
7.76 g/cc
International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Description: DC53 is a general-purpose cold work die and mold steel whose strength and toughness approach those of high-speed steels.Unique Characteristics: Higher hardness (62-63 HRc) than D2 after..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 2.25" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Specific Gravity 7.76 g/cc
7.76 g/cc
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°..