Polymer Property : Specific Gravity = 7.34 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 7.34 g/cc
7.34 g/cc
Meehanite AQ Flake Graphite Cast Iron
Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate..
Specific Gravity 7.34 g/cc
7.34 g/cc
Meehanite GM-60 Flake Graphite Cast Iron
Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a..