Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.22 g/cc | 7.22 g/cc | |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |