Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.19 g/cc | 7.19 g/cc | Calculated |
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |