Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 6.80 g/cc | 6.80 g/cc | |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |
|||
Specific Gravity | 6.80 g/cc | 6.80 g/cc | ASTM D792 |
Ecomass® 4703ZD88 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |