Physical Properties Metric English Comments
Specific Gravity 6.50 g/cc
6.50 g/cc
ASTM D792
Ecomass® 1850ZD88 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Specific Gravity 6.50 g/cc
6.50 g/cc
ASTM D792
Ecomass® 1850ZG90 Metal Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Specific Gravity 6.50 g/cc
6.50 g/cc
ASTM D792
Ecomass® 1850ZG92 Metal Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Specific Gravity 6.50 g/cc
6.50 g/cc
Parker Chomerics CHO-SHIELD® 1091 PRIMER
CHO-SHIELD 1091 is an air-drying liquid coating for enhancing the adhesion of CHO-SHIELD 2001 and 2003 corrosion resistant, electrically conductive coatings to chemically treated aluminum. CHO-SHIEL..