Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 5.70 g/cc | 5.70 g/cc | ASTM D792 |
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform.. |