Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.55 - 5.05 g/cc | 4.55 - 5.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |