Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.70 - 5.00 g/cc | 2.70 - 5.00 g/cc | at 20 degrees Celsius |
Reade Advanced Materials Chromium Trioxide (CrO3) Description: A hexavalent chromium compound and a powerful oxidizing agent. Health effects are limiting applications. Uses: Chromium plating, wood preservation industry, anodizing aluminum, corros.. |
|||
Specific Gravity | 4.90 - 5.00 g/cc | 4.90 - 5.00 g/cc | |
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide Product Description: INHANCE Ti-9000 consists of spherically shaped titanium carbide micro grains. This product is used to make other INHANCE polymer alloys. When incorporated in polymers, unique .. |