Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.95 g/cc | 3.95 g/cc | ASTM D4745 |
3M Dyneon™ CC146/S Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |