Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.52 g/cc | 3.52 g/cc | Part B |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |