Polymer Property : Specific Gravity = 3.36 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 3.36 - 3.41 g/cc
3.36 - 3.41 g/cc
ASTM D792
Isoflon PTFE + 50% Stainless Steel (AISI 316 L) Polytetrafluoroethylene with 50% INOX Stainless Steel
Properties:Improved compression resistance (very low cold flow)Low permeabilityApplications: Dynamic seals operating under high pressure and when chemical resistance is a necessity.Information prov..