Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.33 g/cc | 3.33 g/cc | ASTM D4894 |
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Specific Gravity | 3.33 g/cc | 3.33 g/cc | Part B |
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |