Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.26 g/cc | 3.26 g/cc | Part A |
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr.. |