Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.09 - 3.14 g/cc | 3.09 - 3.14 g/cc | ASTM D792 |
Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for .. |