Polymer Property : Specific Gravity = 2.99 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.99 g/cc
2.99 g/cc
ASTM D792
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6)
Information provided by PolyOne