Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.95 g/cc | 2.95 g/cc | Part A |
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”.. |