Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.88 g/cc | 2.88 g/cc | Part A |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Specific Gravity | 2.88 g/cc | 2.88 g/cc | |
Chesterton 752 Cold Galvanizing Compound Description: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The p.. |