Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.86 g/cc @Temperature 25.0 °C |
2.86 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 4448 CV KIT PARTS A&B Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning |
|||
Specific Gravity | 2.86 g/cc | 2.86 g/cc | Part B |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |
|||
Specific Gravity | 2.86 g/cc | 2.86 g/cc | |
BYK Cloisite® Na+ Nanoclay Cloisite® Na+ is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |