Physical Properties Metric English Comments
Specific Gravity 2.26 g/cc
2.26 g/cc
ASTM D4745
3M Dyneon™ CC503 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% mineral blended with PTFE.Information provided by Dyneon, A 3M Company
Specific Gravity 2.26 - 2.28 g/cc
2.26 - 2.28 g/cc
ASTM D792
Adamas Adalon® 205 PTFE, 15/5% Glass/MoS2 Filled
Information provided by Adamas, HPM
Specific Gravity 2.26 - 2.28 g/cc
2.26 - 2.28 g/cc
ASTM D792
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled
Information provided by Adamas, HPM
Specific Gravity 2.26 g/cc
2.26 g/cc
ASTM D4745
3M Dyneon™ CC203 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% mineral blended with PTFE.Information provided by Dyneon, A 3M Company