Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.19 g/cc | 2.19 g/cc | |
Asahi Glass Fluon® CD090 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Specific Gravity | 2.19 g/cc | 2.19 g/cc | |
Asahi Glass Fluon® CD141 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |